Clear laminating epoxy ?

 
Post new topic   Reply to topic    Northwest Kiteboarding -> Gorge / Portland / Oregon Coast
previous topic :: next topic  
Author Message
florider

Since 17 Oct 2013
10 Posts
north bend,or
 



PostFri Nov 22, 13 9:39 am    Clear laminating epoxy ? Reply with quote

Thinking about laying an extra layer of 6 once glass on the deck of my new FireWire 5'8" alternator. I usually use west system for ding repair, but it cures discolored. Anybody know of a strong clear curing epoxy? I'm over paying 80 bucks for a urine colored finish!

View user's profile Send private message
Scriffler

Since 03 Jul 2005
581 Posts
LYLE
Addicted



PostFri Nov 22, 13 10:58 am     Reply with quote

Buy some special clear hardener from west system. It mixes with regular west system epoxy to leave a perfectly clear finish. I have used it for years to add extra glass layers to weak off the rack surfboards.

View user's profile Send private message
ShiverMeTimbers

Since 26 Feb 2013
381 Posts
Gig Harbor
Obsessed



PostFri Nov 22, 13 11:03 am     Reply with quote

what resin does Firewire use?

View user's profile Send private message
florider

Since 17 Oct 2013
10 Posts
north bend,or
 



PostFri Nov 22, 13 11:30 am     Reply with quote

They use an epoxy resin, not sure which one.
But if west has a clear laminating hardner I'm on it. Thought about trying system three but don't know anything about it. I'll go w/ the easy choice here.
Thanks

View user's profile Send private message
florider

Since 17 Oct 2013
10 Posts
north bend,or
 



PostFri Nov 22, 13 12:51 pm     Reply with quote

Scriffler, do you glass the deck around the rails for strength or just glass the typical heel dent areas?

View user's profile Send private message
Scriffler

Since 03 Jul 2005
581 Posts
LYLE
Addicted



PostFri Nov 22, 13 2:29 pm     Reply with quote

I cut a whole layer of 4 ounce and wrap it around to bottom around rails. Only about a 2 inch wrap. Just make sure you clean the board really well and key it with 100 grit everywhere the glass will be. Use just enough resin to saturate the glass so you don't have too much sanding to get it smooth.

View user's profile Send private message
Clif

Since 18 Dec 2012
4 Posts
Fort Pierce FL
Kook



PostSat Nov 23, 13 1:58 pm     Reply with quote

check out Resin Research products. They make UV resistant resins that a lot of board builders use.

http://www.resinresearch.net/

View user's profile Send private message
bwd

Since 04 Aug 2007
385 Posts

Obsessed



PostSun Nov 24, 13 9:11 am     Reply with quote

+1 for resin research

View user's profile Send private message
Post new topic   Reply to topic    Northwest Kiteboarding -> Gorge / Portland / Oregon Coast All times are GMT - 8 Hours
Page 1 of 1

 
Jump to:  
You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot vote in polls in this forum
You can attach files in this forum
You can download files in this forum